Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 90.0 °C | 194 °F | |
Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Drying Temperature | 90.0 °C @Time 7200 sec |
194 °F @Time 2.00 hour |
|
NatureWorks® Ingeo™ 2003D General Purpose Transparent Extrusion Grade Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed fo.. |
|||
Drying Temperature | 90.0 °C @Time 7200 sec |
194 °F @Time 2.00 hour |
|
Termopol Termoton® K6GA4040A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Drying Temperature | 90.0 °C | 194 °F | |
Pasargad Polymer Peyvand Pasamid 3P-H1150B Nylon 6, 50% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Drying Temperature | 90.0 - 110 °C @Time 14400 - 21600 sec |
194 - 230 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa PA66-ROW Halogen-free, Flame Retardant PA66 Features:Flame retardantHigh mechanical strengthHigh heat resistanceGood electric propertiesNo bloomingApplications:Injection moldingConnectors, linkersRelay, bobbins, plugsHousehold appliance parts.. |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | |
LG Chemical LUCEL MR-310 Low Warpage POM, 10% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | |
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | |
LG Chemical LUCEL N109-AS Antistatic POM, Unreinforced, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latamid 66 H2 K/40 PA 66, 40% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latamid 66 MDT03-01 PA 66 Polyamide 66 (PA66) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Drying Temperature | 90.0 °C | 194 °F | |
LG Chemical LUPOS GP-2200H General Purpose ABS, 20% Glass Fiber Reinforced, High Heat Resistance LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Laticonther 62 CPG/750 PA 6, Glass Fiber Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latilub 66-10T G/30-V0KB1 PA66, 10% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latilub 66-20ST PA66, Silicone/PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). Silicone / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latiohm 57-05 PD01 G/15 PPA, 15% Glass Fiber Reinforced Semiconductive/dissipative product based on Semi-aromatic polyamide (PPA). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by.. |
|||
Drying Temperature | 90.0 - 100 °C @Time 10800 sec |
194 - 212 °F @Time 3.00 hour |
|
LATI Latistat 67-08 PA66, Impact Modified Dissipative product based on Polyamide 66 (PA66), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Drying Temperature | 90.0 - 100 °C | 194 - 212 °F | Predrying Temperature |
Tisan TISLAMID® 6 30% Mineral Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Drying Temperature | 90.0 - 100 °C | 194 - 212 °F | Predrying Temperature |
Tisan TISLAMID® 66 UNR Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Drying Temperature | 90.0 °C | 194 °F | Extrusion |
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Drying Temperature | 90.0 - 100 °C | 194 - 212 °F | Pre-drying Temperature |
Asahi Kasei Xyron® X05516 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
Drying Temperature | 90.0 °C | 194 °F | |
Pasargad Polymer Peyvand Pasamid 3P-M1000B Nylon 6 Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Drying Temperature | 90.0 - 135 °C | 194 - 275 °F | |
Solvay Specialty Polymers Amodel® A-6625 HS BK324 Polyphthalamide, 25% carbon/glass fiber, ESD grade
(discont Amodel A-6625 HS BK324 is a 25% carbon and glass-fiber-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This .. |