Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 71.1 °C | 160 °F | |
PolyOne LubriOne™ ATT-000/5T Black Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
PolyOne LubriOne™ NI-0920063 NATURAL Polyamide 610 (Nylon 610) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Drying Temperature | 71.1 - 76.7 °C | 160 - 170 °F | |
PolyOne LubriOne™ NN-000/15T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
PolyOne LubriOne™ NN-30GF/13T-2S Black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
PolyOne Stat-Tech™ X ST6600-0040 ES FR Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Drying Temperature | 71.1 °C | 160 °F | |
Nilit Polynil® N66-P50N Lubed Nylon 6/6 Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
Polymer Resources PPX-FR1-[color]EN Modified PPO, UL 94 V-0 with HDT of 190 F, Extrusion Grade Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 71.1 - 79.4 °C | 160 - 175 °F | |
PTS SAN-80HF High Flow SAN Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PTS Trimid® N66-1010 Utility Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PTS Trimid® N66-1010L Lubed, Utility Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PTS Trimid® N66-S100HL-BK High Impact Heat Stabilized Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PTS Trimid® N66-SG33-BK 33% Glass Reinforced, High Impact Black Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PTS Trimid® N66-T100 Toughened Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
PolyOne Edgetek® NN-30GF/000 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
PolyOne Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
Polymer Resources PPX-SF2 Modified PPO, Structural Foam Grade, Standard Flow
(Unverified Data**) Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PolyOne Lubri-Tech™ AT-000/5T Black Acetal-Copolymer, PTFE Lubricated
(discontinued **) Preliminary DataDescription/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PolyOne Lubri-Tech™ AT-15CF/5T Acetal-Copolymer, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **)&l Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | 2 hrs |
PolyOne Edgetek® AS-10GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
LTL Color Compounds ColorFast® FRA204 ABS High gloss, excellent impact ABS, V0/5VA-ratedAll information provided by LTL Color Compounders, Inc. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
Ecomass® 720ZD88 Tungsten Filled ABS High Specific GravityTungsten Powder Filled ABSGood ToughnessPlateableInformation provided by Technical Polymers |
|||
Drying Temperature | 71.1 - 82.2 °C @Time 7200 - 14400 sec |
160 - 180 °F @Time 2.00 - 4.00 hour |
|
Entec Hyril® GP355AS Styrene Acrylonitrile Available in North America Features: Copolymer Automotive Specifications: DELPHI M-9565-9 Color: Blue-TransparentForm: PelletsProcessing Method: ExtrusionInformation provided by Entec |
|||
Drying Temperature | 71.1 - 85.0 °C | 160 - 185 °F | or lower with overnight predrying |
AdvanSource Biomaterials ChronoFlex® AL 80A Biodurable Medical Grade Polyurethane ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas.. |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PolyOne Lubri-Tech™ AT-10GF-10KV/000 Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedAramid Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
Polymer Resources PPX-SF1 Modified PPO, Structural Foam Grade, Easy Flow
(Unverified Data**) Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PolyOne Edgetek® AT-10GF/000 FDA Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 71.1 - 79.4 °C | 160 - 175 °F | Average value: 74.4 °C Grade Count:5 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |