Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 50.0 °C @Time 14400 sec |
122 °F @Time 4.00 hour |
|
NatureWorks® Ingeo™ AW 240D Biopolymer for Food Serviceware NatureWorks® PLA polymer AW 240D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed .. |
|||
Drying Temperature | 50.0 - 55.0 °C @Time >=10800 sec |
122 - 131 °F @Time >=3.00 hour |
If stored for longer than 1 year |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Drying Temperature | 50.0 - 149 °C | 122 - 300 °F | Average value: 99.4 °C Grade Count:33 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Drying Temperature | 50.0 - 140 °C | 122 - 284 °F | Average value: 96.1 °C Grade Count:24 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
Drying Temperature | 50.0 - 150 °C | 122 - 302 °F | Average value: 130 °C Grade Count:14 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Drying Temperature | 50.0 - 150 °C | 122 - 302 °F | Average value: 122 °C Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Drying Temperature | 50.0 - 60.0 °C | 122 - 140 °F | |
Kostat BK-STAT BK-STAT is an inherently dissipative polymer incorporated into a variety of resins as a melt additive. The electrical resistivity is reduced by formation of a conductive percolating network in the .. |
|||
Drying Temperature | 50.0 °C | 122 °F | |
Borealis Supersmooth™ LE0500 Crosslinkable Semiconductive Shielding Compound Supersmooth LE0500 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0500 is based on an ethylene butyl acry.. |
|||
Drying Temperature | 50.0 °C | 122 °F | |
Eastman Eastar CN005 Copolyester, High Flow Grade Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit.. |
|||
Drying Temperature | 50.0 °C | 122 °F | |
Eastman Eastar CN015 Copolyester, High Flow Grade with Mold Release Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit.. |
|||
Drying Temperature | 50.0 - 140 °C | 122 - 284 °F | Average value: 102 °C Grade Count:5 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |