Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latigea B01 F1 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latigea B01 I8 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |
|||
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latigea B01 L/07 Bio-Polymer Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.. |
|||
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latigray 37 B01-01 CX/35 Bio-Polymer Radiopaque compound based on Bio-Polymer (PLA, PHB, ...). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latilub 37 B01-02S Bio-Polymer Self-lubricating product based on Bio-Polymer (PLA, PHB, ...). Silicone.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Drying Temperature | <= 40.0 °C | <= 104 °F | |
Trelleborg Horda Cable E8400 Easy Strippable Semiconductive Shielding E8400 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8400 meets the requirements as be.. |
|||
Drying Temperature | <= 40.0 °C | <= 104 °F | |
Trelleborg Horda Cable E8406 Easy Strippable Semiconductive Shielding E8406 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8406 meets the requirements as be.. |
|||
Drying Temperature | <= 40.0 °C | <= 104 °F | |
Trelleborg Horda Cable E8409 Easy Strippable Semiconductive Shielding E8409 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8409 meets the requirements as be.. |
|||
Drying Temperature | <= 40.0 °C | <= 104 °F | |
Trelleborg Horda Cable E8413 Easy Strippable Semiconductive Shielding E8413 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8413 meets the requirements as be.. |
|||
Drying Temperature | <= 40.0 °C | <= 104 °F | |
Trelleborg Horda Cable E8415 Easy Strippable Semiconductive Shielding E8415 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8415 meets the requirements as bel.. |
|||
Drying Temperature | <= 40.0 °C | <= 104 °F | pellets below 200 PPM (Karl Fischer method) |
Trelleborg Horda Cable E8502 Strippable Semiconductive Shielding E8502 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8502 meets the requirements as bel.. |
|||
Drying Temperature | <= 40.0 °C | <= 104 °F | |
Trelleborg Horda Cable E8551 Strippable Semiconductive Shielding E8551 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8551 meets the requirements as bel.. |
|||
Drying Temperature | <= 40.0 °C | <= 104 °F | |
Trelleborg Horda Cable E8560 Strippable Semiconductive Shielding E8560 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8560 meets the requirements as bel.. |
|||
Drying Temperature | <= 40.0 °C | <= 104 °F | |
Trelleborg Horda Cable E8561 Strippable Semiconductive Shielding E8561 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8561 meets the requirements as bel.. |
|||
Drying Temperature | <= 40.0 °C | <= 104 °F | |
Trelleborg Horda Cable E8900 Strippable Semiconductive Shielding E8900 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8900 meets the requirements as be.. |
|||
Drying Temperature | <= 40.0 °C | <= 104 °F | |
Trelleborg Horda Cable E8465 Easy Strippable Semiconductive Shielding E8551 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8551 meets the requirements as bel.. |
|||
Drying Temperature | 40.0 - 60.0 °C @Time 10800 sec |
104 - 140 °F @Time 3.00 hour |
|
LATI Latigea B02 H6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Improved thermal stability. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latimass 37 B01-01 D025 Bio-Polymer Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latigea B01 I6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |