Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 180 - 204 °C | 356 - 400 °F | Average value: 196 °C Grade Count:5 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Drying Temperature | 180 °C | 356 °F | |
Lubrizol Estane® ZHF 90AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 90AT0 TPU is a clear, glossy, zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding TPU properties.Uses: Cable jacket and tube/hos.. |
|||
Drying Temperature | 180 °C | 356 °F | |
ExxonMobil Santoprene® 8221-75M300 Thermoplastic Elastomer A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and .. |