Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa PBT-G30 30% Glass Fiber Reinforced PBT Features:Good size stabilityHigh mechanical propertiesHigh heat resistanceExcellent balance propertiesApplications:Injection moldingApplication partsAuto handleDoor latchE & E partsInformation Provi.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa PBT-RG30 Flame Retardant, 30% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa PBT-T15 15% Mineral Filled PBT Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Rear Barrel Temperature | 200 - 240 °C | 392 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT 1155D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUCON 6080EX ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio.. |
|||
Rear Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Injection Molding |
LG Chemical LUPOY EC5000AF PC/ABS, Flame Residence Description: Injection Molding, PC/ABS, Flame Residence, Anti-StaticApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 68928-70-1Information provided by LG Chemical |
|||
Rear Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Injection Molding |
LG Chemical LUPOY GN5001SF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa PBT-G15 15% Glass Fiber Reinforced PBT Features:Good size stabilityHigh mechanical propertiesHigh heat resistanceExcellent balance propertiesApplications:Injection moldingApplication partsAuto handleDoor latchE & E partsInformation Provi.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa PBT-RG002 Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa PBT-RG151 Flame Retardant, 15% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesExcellent size stabilityNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInforma.. |
|||
Rear Barrel Temperature | 225 - 240 °C | 437 - 464 °F | Injection Molding |
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant Description: Injection Molding, PC/ABS, Halogen Free Flame RetardantApplication: Industrial / IT productCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Rear Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Injection Molding |
LG Chemical LUPOY GN5009F PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 190 - 240 °C | 374 - 464 °F | Injection |
Inno-Comp INNOPOL® CS 1-2120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL CS 1-2120 AP is a 20 % talc filled compound based on polypropylene homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 1-2120 AP is recommended especially.. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Samyang Tribit® 1500 Polybutylene Terephthalate Characteristics:Medium viscosityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samy.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 30% Mineral Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 Flame Retardant (V0) Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Zone 1 |
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Zone 1 |
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Zone 1 |
Eurostar Staramide BG6ST43 PA6, 30% Glass Fiber Filled, Impact Modified, Injection Molded BG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Beijing Chemical Industry KAIFA® MN201-G20 Nylon 66 Resin 20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |