Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 220 - 235 °C | 428 - 455 °F | Start Point: 230°C |
Kingfa MAC-501 Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Rear Barrel Temperature | 220 - 235 °C | 428 - 455 °F | Start Point: 230°C |
Kingfa MAC-601 DY Modified 60/40 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelPower toolComputer and acce.. |
|||
Rear Barrel Temperature | 215 - 235 °C | 419 - 455 °F | Injection Molding |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 205 - 235 °C | 401 - 455 °F | Injection Molding |
LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 215 - 235 °C | 419 - 455 °F | Injection Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 225 - 235 °C | 437 - 455 °F | Injection Molding |
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an.. |
|||
Rear Barrel Temperature | 225 - 235 °C | 437 - 455 °F | Injection Molding |
LG Chemical LUMAX GP5200B PBT+ABS+GF20% Description: Injection Molding Grade, PBT+ABS+GF20%, General PurposeApplication: E&E (Speaker Frame)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 9003-54-7Information provided by LG Chemical |
|||
Rear Barrel Temperature | 225 - 235 °C | 437 - 455 °F | Injection Molding |
LG Chemical LUMAX GP5306F PBT+ABS+GF30%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF30%, Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4Information provided by LG .. |
|||
Rear Barrel Temperature | 225 - 235 °C | 437 - 455 °F | |
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Rear Barrel Temperature | 225 - 235 °C | 437 - 455 °F | Injection Molding |
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
Rear Barrel Temperature | 225 - 235 °C | 437 - 455 °F | |
LG Chemical LUMAX HR-5306F Heat Resistant PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Rear Barrel Temperature | 220 - 235 °C | 428 - 455 °F | Injection Molding |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 235 °C | 428 - 455 °F | Injection Molding |
LG Chemical LUPOS GP2205 SAN+GF20%, General Purpose Feature: Injection Molding, SAN+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 235 °C | 428 - 455 °F | Injection Molding |
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance Feature: Injection Molding, ABS+GF20%, General Purpose, Heat ResistanceApplication: Electric & Electronic (Housing, Components)Information provided by LG Chemical |
|||
Rear Barrel Temperature | 230 - 235 °C | 446 - 455 °F | Injection Molding |
LG Chemical Lupox® GP1000H PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 230 - 235 °C | 446 - 455 °F | Injection Molding |
LG Chemical Lupox® GP1000M PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 230 - 235 °C | 446 - 455 °F | Injection Molding |
LG Chemical Lupox® GP1000S PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 230 - 235 °C | 446 - 455 °F | Injection Molding |
LG Chemical Lupox® GP1000SB PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 230 - 235 °C | 446 - 455 °F | Injection Molding |
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Rear Barrel Temperature | 225 - 235 °C | 437 - 455 °F | |
LG Chemical Lupox® GP-2000 General Purpose PBT, Unreinforced, Medium Viscosity LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Rear Barrel Temperature | 225 - 235 °C | 437 - 455 °F | |
LG Chemical Lupox® PBT-GP-1000 High Flow PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 225 - 235 °C | 437 - 455 °F | |
LG Chemical Lupox® SV-1080 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Rear Barrel Temperature | 220 - 235 °C | 428 - 455 °F | Injection Molding |
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 218 - 235 °C | 425 - 455 °F | |
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced Features: Heat Stabilized; Warp Resistant Forms: Pellets Additive: Heat Stabilizer Automotive Specifications: GM GMP.PA6.011Information Provided by Teknor Apex |
|||
Rear Barrel Temperature | 218 - 235 °C | 425 - 455 °F | |
Teknor Apex Chemlon® 253 Nylon 6, Toughened Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation .. |
|||
Rear Barrel Temperature | 216 - 235 °C | 420 - 455 °F | |
Teknor Apex Chemlon® 275H Nylon 6, Copolymer, Impact Modified Notes: Very high impact and elongation, low flexural modulus material for tubing and wire jacketing applications requiring a soft, flexible product; FMVSS Flammability: Passes, FMVSS 302Processing M.. |
|||
Rear Barrel Temperature | 218 - 235 °C | 425 - 455 °F | |
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio.. |
|||
Rear Barrel Temperature | 218 - 235 °C | 425 - 455 °F | |
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor.. |
|||
Rear Barrel Temperature | 218 - 235 °C | 425 - 455 °F | |
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S.. |