Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene.. |
|||
Rear Barrel Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ OM 6059-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6059-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ OM 6240-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6240-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6258-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ OM 6258-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6258-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ OM 6275-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6275-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. New Prod.. |
|||
Rear Barrel Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE) Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p.. |
|||
Rear Barrel Temperature | 196 - 204 °C | 385 - 399 °F | |
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE) Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat .. |
|||
Rear Barrel Temperature | 166 - 204 °C | 331 - 399 °F | |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 1983 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Color Stable, Custom colors, UL94 HB at 0.060 for all colorsApplications: Suitable for extrusion or injection molding processes requiring.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 240 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact with good flexural stiffness, Custom colorsApplications: Injection molding, Small appliances, Photographic equipmentPerformance grades of polystyrene are engineered to have spe.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 271 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Excellent balance of stiffness, heat resistance, and impact properties, Custom colorsApplications: Injection molding and extrusion, Applications requiring strength and durability where custom colori.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 474 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Alternative to engineering resinsPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. N.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 1552 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Easy processing, High modulus, Improve stress whitening, Custom colorsApplications: Injection molding, Office furniture, Electronic media, Photographic equipmentPerformance grades of polystyrene are.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 850 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Custom colorsApplications: Injection molding or extrusion, Suitable replacement for some engineering resins, Toys, Packaging, Business eq.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 765 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, High impact, Color stable, Custom colorsApplications: High flow, multi-purpose injection molding grade where color stability is a requirement, Toys, Appliance, Computer peripheralsPerform.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 782 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Custom colorsApplications: Multi-purpose injection molding where custom color is a requirement, Toys, Appliance, Computer peripheralsPerformance grades of polystyrene are engineered to ha.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 8077 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova Styrosun® 6600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 8047 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 8049 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High gloss at 60°=95; at 20°C=90, Improved scuff resistance, Custom colorsApplications: Injection molding, Cost effective replacement for some ABS applications, Excellent for applications where hi.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova Zyntar® 702 High Performance Flame Retardant Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Gas-assist injection moldingThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in laboratory flame tests. L.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova Zyntar® 351 High Performance Flame Retardant Polystyrene
(discontinued **) High Vicat and heat reflection temperature, Custom colorsApplications: Injection molding, Gas-assist injection molding, Structural foam, TV cabinets, Electronic enclosuresThis is an impact grade of .. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |