Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling .. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical AF312 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HI110 ABS, High Impact, Chemical Resistance Feature: Injection Molding, High Impact, Chemical ResistanceApplication: Edge of Furniture ApplicationsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HI153 ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HIPS 406AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical HIPS 460AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical KEYFLEX TO1192A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical LI911 ASA Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical RX710 ABS, High Impact, Chemical Resistance to HCFC Feature: Injection Molding, Chemical Resistance to HCFC, High ImpactApplication: Refrigerator Dispensor & HomebarCAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
Huntsman AVALON® 92 AB Thermoplastic Polyurethane Introduction: AVALON 92 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 92 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
Huntsman AVALON® 95 AB Thermoplastic Polyurethane Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | c |
LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Rear Barrel Temperature | 170 - 200 °C | 338 - 392 °F | |
Elastron® V TPV Elastomer Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with v.. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical KEYFLEX TO1088AV Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0Information provided by LG Chemical |
|||
Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
Huntsman AVALON® 95 ABR Thermoplastic Polyurethane Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
LG Chemical KEYFLEX TO1075AR Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical |