Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne OnFlex™ HFFR 360-0185 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 360-0185 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - Non-halogen flame re.. |
|||
Rear Barrel Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne OnFlex™ HFFR 361-0190 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 361-0190 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - UL 94 HB compliantPu.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 379 °F | |
PolyOne Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-43N is a unique TPE designed for the demanding requirements of gaskets and stoppers used in healthcare and food packaging applications. New Product. Commercial specifications hav.. |
|||
Rear Barrel Temperature | 160 - 193 °C | 320 - 379 °F | |
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV.. |
|||
Rear Barrel Temperature | 166 - 193 °C | 331 - 379 °F | |
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Rear Barrel Temperature | 166 - 193 °C | 331 - 379 °F | |
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Rear Barrel Temperature | 182 - 193 °C | 360 - 379 °F | |
PolyOne Versaflex™ OM 9-801N Thermoplastic Elastomer (TPE) Versaflex™ OM 9-801N is designed for overmolding onto a wide variety of substrates including PC, ABS, PC/ABS, HIPS, PPO, acetal, acrylic and copolyester. - Bonds to a Variety Of Substrates - Rubber.. |
|||
Rear Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Rear Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Rear Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Rear Barrel Temperature | 154 - 193 °C | 309 - 379 °F | |
PolyOne Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3226-1000-03 is an easy processing TPE designed for general purpose applications. It is suitable for injection molding, extrusion, blow molding and thermoforming processes. - Dry Feel - .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 379 °F | |
Ineos Nova Zyntar® F7080 Developmental Flame Retardant Polystyrene
(discontinued **) Features: General purpose non-Deca based resin (does not combine with Decabromodiphenyloxide)Good indoor UV light color stability(grey colors)UL94 V-0 @ 1.5 mm for all colors Good aesthetics for inj.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 379 °F | |
Ineos Nova Zyntar® F7080UV Developmental Flame Retardant Polystyrene
(discontinued **) Features: General purpose non-Deca based resin (does not combine with Decabromodiphenyloxide)Good indoor UV light color stability(grey colors)UL94 V-0 @ 1.5 mm for all colors Good aesthetics for inj.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 379 °F | |
Ineos Nova Zyntar® F7120 Developmental Flame Retardant Polystyrene
(discontinued **) Features: High flow for thin wall partsGood balance of physical propertiesUL94 V-0 @ 1.5 mm for black color Good aesthetics for injection molding Applications:Large television cabinetsConsumer elect.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 379 °F | |
Ineos Nova Zyntar® 7001 High Performance Flame Retardant Polystyrene
(discontinued **) Super high flow, Reduced processing temperatures, Reduced processing time, Improved aesthetics, Custom colorsApplications: Injection molding, Gas-assist injection molding, Hard to fill cavities, suc.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 379 °F | |
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 379 °F | |
Ineos Nova Zyntar® 7000 Flame Retardant Polystyrene Features:General purpose workhorse resinGood flow for injection moldingUL94 V-0 @ 1.5 mm for all colors UL94 5VA rating FOAMED @ 4.6 mm, 0.87-1.07 g/cc density, natural colorCustom colors availableA.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 379 °F | |
Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |