Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 168 - 174 °C | 335 - 345 °F | |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 168 - 174 °C | 335 - 345 °F | |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 168 - 174 °C | 335 - 345 °F | |
Polymer Resources AC-GP2-[color]-3 Acetal Copolymer, Medium Flow, General Purpose Molding, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 168 - 174 °C | 335 - 345 °F | |
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 168 - 174 °C | 335 - 345 °F | |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 168 - 174 °C | 335 - 345 °F | |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 168 - 174 °C | 335 - 345 °F | |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 168 - 174 °C | 335 - 345 °F | |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Walled Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |