Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC/TP-GP1-[color]-3 PC Polyester, High Impact, Good Chemical Resistance, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC-GP4-[color]-3 Polycarbonate, UV-stabilized, Easy Flow Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow Polycarbonate, FDA-compliant Feedstocks, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-GP1 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-GP2 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-GP4 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Rear Barrel Temperature | 249 - 260 °C | 480 - 500 °F | |
Ravago Manufacturing Americas Hybrid S451H Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Flame Retardant High Flow RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)& Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Oxford Polymers PC C20-000 Clear PC Product Description: Amorphous, Unreinforced Polycarbonate injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Pigment onlySpecial Characteristics: Easy fl.. |
|||
Rear Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized Nylon 6, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade PC/ABS Alloy, General Purpose, Low Gloss GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Polymer Resources PC-UV4-[color]-1 Polycarbonate, UV-stabilized, Easy Flow with Mold Release Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Mitsubishi Iupilon® S3000UR 16.5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
MRC Polymers EMAREXâ„¢ 300 GF43 Nylon 6, 43% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Samyang Trirex® PC-3022U 15 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Clariant 6008 L Nylon 6, High Impact, Injection Molding Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Clariant PA213M40 Nylon 6, 40% Mineral Reinforced, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-GP4-WR Modified PPO, Wear Resistant with HDT of 215 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |