Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources PPX-SF1 Modified-PPO, Structural Foam Grade, Flame Retardant, Easy Flow Modified-Polyphenylene Oxide, Structural Foam Grade, Easy FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechani.. |
|||
Rear Barrel Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec.. |
|||
Rear Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Rear Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Rear Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Rear Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Rear Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Rear Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 232 - 243 °C | 450 - 470 °F | |
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources NY6-G43-[color]-H Nylon 6, 43% Glass Reinforced, Heat Stabilized Nylon 6, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Rear Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources NY6-M25G15 Nylon 6, 25% Mineral, 15% Glass Reinforced Nylon 6, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gra.. |
|||
Rear Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Rear Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources NY6-M40 Nylon 6, 40% Mineral Filled Nylon 6, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested .. |
|||
Rear Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources NY6-M40-[color]-H Nylon 6, 40% Mineral Filled, Heat Stabilized Nylon 6, 40% Mineral Filled, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Rear Barrel Temperature | 232 - 243 °C | 450 - 470 °F | |
Ravago Manufacturing Americas Hybrid S464LG Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color: Natural, Chry.. |
|||
Rear Barrel Temperature | 232 - 254 °C | 450 - 490 °F | |
Ravago Manufacturing Americas Hylex® P1325L Polycarbonate, UV Stabilized, High Flow, Mold Release Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Rear Barrel Temperature | 232 °C | 450 °F | |
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade ALATHON H4250 is a high-flow “freezer†grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p.. |
|||
Rear Barrel Temperature | 232 °C | 450 °F | |
LyondellBasell Alathon® H4620 High Density Polyethylene, Injection Molding Grade Alathon H4620 is a medium-flow resin that exhibits good cold temperature impact performance, enhanced processing and thermal stability. Typical applications are thinner-walled parts that require che.. |
|||
Rear Barrel Temperature | 232 °C | 450 °F | |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Rear Barrel Temperature | 232 °C | 450 °F | |
LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, c.. |
|||
Rear Barrel Temperature | 232 °C | 450 °F | |
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a.. |
|||
Rear Barrel Temperature | 232 °C | 450 °F | |
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade ALATHON M5352 is a high density copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good proces.. |
|||
Rear Barrel Temperature | 232 °C | 450 °F | |
LyondellBasell Alathon® M5372 High Density Polyethylene ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. .. |
|||
Rear Barrel Temperature | 232 °C | 450 °F | |
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include case.. |
|||
Rear Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Star Plastics PC/PBT7804 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 232 - 243 °C | 450 - 470 °F | |
Entec Hylox® 9030 PBT, 30% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Rear Barrel Temperature | 232 - 243 °C | 450 - 470 °F | |
Entec Hylox® 9230BK PBT, 30% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Rear Barrel Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources PPX-SF1 Modified PPO, Structural Foam Grade, Easy Flow
(Unverified Data**) Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Rear Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc. |