Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F38-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Electrical housingsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F43-01B 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Drip trayFunctional supportsA/C housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT4200-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT7013-720UV Thermoplastic Polyolefin, UV Stabilized, XTM Dark Sandstone Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT7013-721UV Thermoplastic Polyolefin, UV Stabilized, XDV Dark Slate Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC30P200-01 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC35P200-01UV 35% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, General Purpose Black Applications: BracketsStructural componentsHeadlamp housingsWindow frameInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products RCC233-01 33% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: Fender linersSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | >= 204 °C | >= 400 °F | |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F35-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Interior trimUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products G30P100-00 30% Glass Fiber Reinforced Polypropylene, Natural Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
PlastiComp Complet® LCF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 40% carbon fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP525-283 30% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, RK8 Medium Camel Applications: Automotive interior applicationsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas.. |
|||
Rear Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas.. |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Fiberfil® J-69/10/E High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Fiberfil® J-69/30/E High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Fiberfil® J-69/30/E/M High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 204 - 238 °C | 400 - 460 °F | |
LTL Color Compounds ColorFast® PBA1000 PBT/ABS Alloy PBT/ABS alloy with excellent physical properties and chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Fiberfil® J-69/40/E High performance polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO TF 1120 HP Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 1120 HP is a 20% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lightin.. |
|||
Rear Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO TF 2104 GP Recycled Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 2104 GP is a 20% talc reinforced polypropylene homopolymer made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden products.D.. |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent
soft touch feel a.. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products CC30P100-00 30% Calcium Carbonate Reinforced Polypropylene, Natural Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |