Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
Multibase Multi-Pro® 2510 XGW Polypropylene Mineral Filled, 27% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT2202-732UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Box top railTail gate linerExterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4500-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Automotive componentsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4700-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products G13P100-00 13% Glass Fiber Reinforced Polypropylene, Natural Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products G13P100-553UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 501F) Dark Smoke Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products G13P100-598UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (NH-293L) Seagull Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products GC15P200-00 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP514-182 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP514-197 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 848 Black Applications: Mirror housingsInterior trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP521-231 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 173B Navy Blue Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products M12P250-01 12% Mica Reinforced Polypropylene Copolymer, Black Applications: Filler panelsHVAC ductsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products M15P100-01A 15% Mica Reinforced Polypropylene, Black Applications: Fan shroudsAir ductsElectronicsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products T12P600-01BG 12% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: Flipper panelClose out panelSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 193 °C | 380 °F | |
PTS Trilac® ABS-HS5500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 193 °C | 380 °F | |
PTS Trilac® ABS-RC3000 Recycled Black ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 193 °C | 380 °F | |
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP522-286 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZUCA Medium Graphite Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products M15P101-01 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 210 °C | 380 - 410 °F | |
Fiberfil® J-60/GB/20 Polypropylene Homopolymer, 20% Glass beads Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Kraton® G7820 GU-N (SEBS) Compound Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Rear Barrel Temperature | 193 °C | 380 °F | |
Chi Mei Polylac® PA-747 ABS High impact |
|||
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 193 - 204 °C | 380 - 400 °F | |
Kraton® G7720 GI-N (SEBS) Compound Description: Kraton G7720 GI-N is an easy processing, general purpose 57 Shore a hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |