Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6258-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP 1049 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP 1249D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1301A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1580-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1698 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1775D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1862R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1871 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2103 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2112 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2120 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2156E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2215 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1855J Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2664A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2820M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3445DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 3480N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion |
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Rear Barrel Temperature | 182 - 216 °C | 360 - 420 °F | |
CTC X-PRO CTC PP 2025 Polypropylene Impact Copolymer X-PRO PP 2025 is an impact, polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Rear Barrel Temperature | 182 - 216 °C | 360 - 420 °F | |
CTC X-PRO CTC PP 5002 Polypropylene Copolymer X-PRO PP 5002 is a polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Rear Barrel Temperature | 182 - 216 °C | 360 - 420 °F | |
CTC X-PRO PP 2021 Polypropylene Impact Copolymer X-PRO PP 2021 is an impact, polypropylene copolymer. It has general purpose applications.Data provided by Composite Technologies (CTC). |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1875UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-2890M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Rear Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
Ineos Nova 8047 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app.. |
|||
Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
Teknor Apex Monprene® MP-1875HF Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |