Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigm.. |
|||
Rear Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Rear Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-GP1-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Rear Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-GP1-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Low Flow Polycarbonate, 5% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Rear Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Rear Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | Injection Molding |
LG Chemical LUCON CP510F PC/ABS+CNT Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, High Flow, Good ProcessabilityApplication: Copy Machine Paper GuideCAS No. 103598-77-2 and 7440-44-0Information provided b.. |
|||
Rear Barrel Temperature | 282 - 310 °C | 540 - 590 °F | |
Wellman Wellamid® GF60-66/6 XE-N 60% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher .. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R533T Nylon 66, Translucent, 33% Glass Filled, Dry as Molded Vydyne® R533T is a translucent 33% glass-reinforced PA66 resin designed specifically for use in power-steeing reservoirs dn other applications where chemical resistance, whiteness and transmittance.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl.. |
|||
Rear Barrel Temperature | 290 - 310 °C | 554 - 590 °F | |
Unitika P-3001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f.. |
|||
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |