Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release ROHS Compliant.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 232 - 274 °C | 450 - 525 °F | |
Star Plastics PC/ABSQX7002 Molding Grade PC/ABS High Flow Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 238 - 274 °C | 460 - 525 °F | |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
Star Plastics PC20NBR Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
Star Plastics PC721HFR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
Star Plastics PC721HFR Molding Grade PC High Flow with Release Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
Star Plastics PC7523R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
CTC X-PRO PP 100 P1015 Polypropylene Homopolymer X-PRO PP 1015 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |