Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 190 - 220 °C | 374 - 428 °F | Start Point: 210°C |
Kingfa HR-528 Modified ABS Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Start Point: 215°C |
Kingfa LONOY 1300 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical KEYFLEX BT 5035D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Modulus, Black ColorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical LI951 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Radiator Grill, Side Mirror)CAS: 26299-47-8Information provided by LG Chemical |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical LUCON PS4200 ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Good Dimensional Stability, Low WarpageApplication: IC TrayCAS No. 9003-56-9, 12001-26-2 and 7440-44-0Information provided by LG Ch.. |
|||
Rear Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUPOL GP-1000FA General Purpose Polypropylene, High Impact, Flame Retardant, Non-Bleed LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUPOL HG-3200 High Gloss Polypropylene, 20% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUPOL HG-3250 High Gloss Polypropylene, 25% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Rear Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection Molding |
LG Chemical XR440 ABS, Low Emission High Heat ABS Feature: Injection Molding Grade, Low Emission High Heat ABSApplication: Automotives Interior housingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection Molding |
LG Chemical XR490 ABS, Heat Resistance, Low Emission Feature: Injection Molding, Heat Resistance, Low EmissionApplication: Automotives Interior Housing (Glove Box Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG C.. |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUPOL SO-5202P High Impact Polypropylene, 20% Polymer Alloy LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUPOL TE-5102 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | H1 |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Unitika AX-1500W Dry Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis.. |
|||
Rear Barrel Temperature | 210 - 220 °C | 410 - 428 °F | |
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin 10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Rear Barrel Temperature | 210 - 220 °C | 410 - 428 °F | |
Beijing Chemical Industry KAIFA® HN301-G30 PA6 Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Rear Barrel Temperature | 195 - 220 °C | 383 - 428 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Rear Barrel Temperature | 195 - 220 °C | 383 - 428 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Rear Barrel Temperature | 190 - 220 °C | 374 - 428 °F | Pipe Extrusion |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Rear Barrel Temperature | 195 - 220 °C | 383 - 428 °F | Tube Extrusion |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Rear Barrel Temperature | 210 - 220 °C | 410 - 428 °F | |
Beijing Chemical Industry KAIFA® HN201-G10 PA6 Resin 10% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Rear Barrel Temperature | 195 - 220 °C | 383 - 428 °F | Tube Extrusion |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Rear Barrel Temperature | 170 - 220 °C | 338 - 428 °F | Injection or Extrusion |
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec.. |
|||
Rear Barrel Temperature | 195 - 220 °C | 383 - 428 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Rear Barrel Temperature | 195 - 220 °C | 383 - 428 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Rear Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUPOL GP-2201F General Purpose Polypropylene, 20% Glass Fiber Reinforced, Flame Retardant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |