Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
Multibase Multi-Pro® 0612 CW Polypropylene Calcium carbonate filler, 6% filer by weightForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
Multibase Multi-Pro® 2518 CU Polypropylene Calcium Carbonate Filler, 25% by weight.Features:Gloss, High Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT1001-74 Thermoplastic Polyolefin, Non-UV Stabilized, DX9 Black Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT2400-647UV Thermoplastic Polyolefin, UV Stabilized, 8798NM Grey Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT2600-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Interior trimSplash shieldsStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P100-00 Polypropylene, Natural Applications: Automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P100-01 Polypropylene Homopolymer, Black Applications: Wire harnessesTrim componentsUnderhood applicationsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P252-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P256-01 Polypropylene Copolymer, Black Applications: Door/trunk scuffConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or.. |
|||
Rear Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3480N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Rear Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Rear Barrel Temperature | 210 - 216 °C | 410 - 420 °F | |
Elastocon TPE Technologies Elastocon® STK60 Thermoplastic Elastomer Elastocon® STK60 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60 is FDA compliant and well s.. |
|||
Rear Barrel Temperature | 210 - 216 °C | 410 - 421 °F | |
Elastocon TPE Technologies Elastocon® STK60X Thermoplastic Elastomer Elastocon® STK60X thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60X is well suited for consume.. |
|||
Rear Barrel Temperature | 210 - 216 °C | 410 - 420 °F | |
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer.. |
|||
Rear Barrel Temperature | 182 - 216 °C | 360 - 420 °F | |
CTC SunPro® SP 200 P 3085 Polypropylene Copolymer SunPro® SP 200 P 3085 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM.PP... |
|||
Rear Barrel Temperature | 182 - 216 °C | 360 - 420 °F | |
CTC X-PRO CTC PP 5002 Polypropylene Copolymer X-PRO PP 5002 is a polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Rear Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO TF 1113 HP Polypropylene Homopolymer, 13% Talc Filled X-PRO TF 1113 HP is a 13% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lightin.. |
|||
Rear Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO TF 1120 HP Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 1120 HP is a 20% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lightin.. |
|||
Rear Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO TF 1140 HP Polypropylene Homopolymer, 40% Talc Filled X-PRO TF 1140 HP is a 40% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, HVAC, and lawn .. |
|||
Rear Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO TF 2104 GP Recycled Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 2104 GP is a 20% talc reinforced polypropylene homopolymer made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden products.D.. |
|||
Rear Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Rear Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Rear Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex.. |
|||
Rear Barrel Temperature | 177 - 216 °C | 350 - 420 °F | Injection Molding |
Teknor Apex Sarlink® 3439DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |