Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Rear Barrel Temperature | 154 - 193 °C | 309 - 379 °F | |
PolyOne Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3226-1000-03 is an easy processing TPE designed for general purpose applications. It is suitable for injection molding, extrusion, blow molding and thermoforming processes. - Dry Feel - .. |
|||
Rear Barrel Temperature | 177 - 193 °C | 350 - 380 °F | |
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Rear Barrel Temperature | 177 - 193 °C | 350 - 380 °F | |
Teknor Apex Flexalloy® 9100-65 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® OBC 2581B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® OBC 4565A Thermoplastic Elastomer Uses: Flexible Grips; Overmolding Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion; Extrusion; Injection Molding Injection .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® OBC 4876N Thermoplastic Elastomer Uses: Flexible Grips; Overmolding; Soft Touch Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1081A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1140E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1154A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1336A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1377A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1472A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1524F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1686D Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1934G Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Connectors; Wire Jacketing; Wire and Cable Applications Agency Ratings: UL 1581Forms: Pellets Proces.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2535F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2563A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2572A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-3260R Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-355 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-3954-50 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-83-F912-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-8712R Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-86-K986T-98 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-8732R Thermoplastic Elastomer Notes: RoHS Compliant Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstri.. |
|||
Rear Barrel Temperature | 177 - 193 °C | 350 - 380 °F | |
Elastocon TPE Technologies Elastocon® 8078B Thermoplastic Elastomer Elastocon® 8078B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078B is well suited for consumer goods a.. |
|||
Rear Barrel Temperature | 182 - 193 °C | 360 - 380 °F | |
Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant Aromatic Polyether BasedData provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 177 - 193 °C | 350 - 380 °F | |
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Rear Barrel Temperature | 177 - 193 °C | 350 - 380 °F | |
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |