Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 166 - 182 °C | 331 - 360 °F | |
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds.. |
|||
Rear Barrel Temperature | 166 - 182 °C | 331 - 360 °F | |
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE) Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 .. |
|||
Rear Barrel Temperature | 166 - 182 °C | 331 - 360 °F | |
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE) Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough.. |
|||
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
Polymer Resources ABS-FR Flame Retardant ABS Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch.. |
|||
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and.. |
|||
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
Polymer Resources ABS-FR1 ABS, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant Contains UV absorber.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 160 - 182 °C | 320 - 360 °F | |
PolyOne Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Rear Barrel Temperature | 160 - 182 °C | 320 - 360 °F | |
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Rear Barrel Temperature | 166 - 182 °C | 331 - 360 °F | |
PolyOne Dynaflex™ G7736-1 Thermoplastic Elastomer (TPE) Dynaflex™ G7736-1 is a general purpose compound designed to provide easy processing and a good surface finish. - Good Aesthetics - Good Ozone/UV Stability - High Flow for Thin-Wall Parts - Overmold.. |
|||
Rear Barrel Temperature | 160 - 182 °C | 320 - 360 °F | |
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Rear Barrel Temperature | 177 - 182 °C | 350 - 360 °F | |
Green Dot Terratek® SC 50 Polypropylene - Wheat Starch Biocomposite Terratek® SC 50 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 50 contains 50% wheat starch by weight, however, a range of properties can be achie.. |
|||
Rear Barrel Temperature | 177 - 182 °C | 350 - 360 °F | |
Green Dot Terratek® SC 65 Polypropylene - Wheat Starch Biocomposite Terratek® SC 65 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 65 contains 65% wheat starch by weight, however, a range of properties can be achie.. |
|||
Rear Barrel Temperature | 177 - 182 °C | 350 - 360 °F | |
Green Dot Terratek® WC 100300 Polypropylene - Pine Fiber Composite Terratek® WC 100300 is a proprietary blend of pine wood fiber and reprocessed polypropylene for injection molding applications. WC 100300 contains 30% wood fiber by weight, however, a range of pr.. |
|||
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
LTL Color Compounds ColorFast® FRA202 General Purpose ABS General purpose V0/5VA-rated ABSAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
LTL Color Compounds ColorFast® FRA203 ABS Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
LTL Color Compounds ColorFast® FRA204 ABS High gloss, excellent impact ABS, V0/5VA-ratedAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
LTL Color Compounds ColorFast® FRA205 ABS Flame-retarded V0, high gloss ABS with superior UV stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
Kraton® D2104 DI-N (SBS) Compound Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D.. |
|||
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
Kraton® D2109 DS-N (SBS) Compound Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
Kraton® D2109 DS-W (SBS) Compound Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Rear Barrel Temperature | 166 - 182 °C | 330 - 360 °F | |
Star Plastics ABS450FR Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 149 - 182 °C | 300 - 360 °F | |
Star Plastics ABSFR1 Molding Grade ABSFR Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 149 - 182 °C | 300 - 360 °F | |
Star Plastics ABSFR2 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 160 - 182 °C | 320 - 360 °F | |
Clariant CA9000NAT` Acetal Copolymer Data provided by Clariant Masterbatches |