Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
Parker Chomerics PREMIER™ A240-FRHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Rear Barrel Temperature | 255 - 275 °C | 491 - 527 °F | Start Point: 265°C |
Kingfa PA66-RG001 Flame Retardant PA66 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesNo bloomingApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation Provided by Kingf.. |
|||
Rear Barrel Temperature | 255 - 275 °C | 491 - 527 °F | Start Point: 265°C |
Kingfa PA66-RG301 Flame Retardant, 30% Glass Fiber Reinforced PA66 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsInformation Provided by Kingfa Sci. & Tech.. |
|||
Rear Barrel Temperature | 255 - 280 °C | 491 - 536 °F | Injection Molding |
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | Injection Molding |
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical |
|||
Rear Barrel Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
LG Chemical LUMID GP1200A(W) PA6, Medium Viscosity Feature: Injection Molding, PA6, Medium ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Rear Barrel Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
LG Chemical LUMID GP1300A(W) PA6, High Viscosity Feature: Injection Molding, PA6, High ViscosityApplication: Automotive PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
LG Chemical LUPOY GP-1000 General Purpose Modified PC, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
LG Chemical LUPOY HI-1002 High Impact Modified PC, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
LG Chemical LUPOY GP-1006F General Purpose Modified PC, Unreinforced, Weather Resistant, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Rear Barrel Temperature | 255 - 265 °C | 491 - 509 °F | |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Rear Barrel Temperature | 255 - 265 °C | 491 - 509 °F | |
Unitika A3130 PA6, 35% Mineral Reinforced, Dry Information provided by Unitika Ltd. |