Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 220 °C | 428 °F | |
NYCOA 2084 HS PA 6 lubricated flexible tubing and conduitInformation provided by NYCOA, Inc. |
|||
Rear Barrel Temperature | 220 °C | 428 °F | |
NYCOA 27/440KNF Glass Filled Nylon 6 44% glass filled, heat stabilized nylon 6Information provided by NYCOA, Inc. |
|||
Rear Barrel Temperature | 220 °C | 428 °F | |
NYCOA 400 PA 6 nucleated general molding gradeInformation provided by NYCOA, Inc. |
|||
Rear Barrel Temperature | 220 °C | 428 °F | |
NYCOA 578 PA 6 very high viscosity molding & extrusion grade for tubing, pipes, film and tapesInformation provided by NYCOA, Inc. |
|||
Rear Barrel Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa MAC-751 HF PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa PBT-RG152 Flame Retardant, 15% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesHigh glossyGood surfaceNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInformation Provided by Kingfa S.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa PBT-RG301 Flame Retardant, 30% Glass Fiber Reinforced PBT Features:Flame retardantHigh mechanical strengthHigh heat resistanceGood electric propertiesNo bloomingApplications:Injection moldingHousehold appliance partsBobbinLighting partsRelayLinkerInformati.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUCON 6080EX ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio.. |
|||
Rear Barrel Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 235 °C | 428 - 455 °F | Injection Molding |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUPOY GN5001RFT PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUPOY GN5008HF PC/ABS, Halogen Free Flame Retardant, High Impact Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: E&E (OA, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUPOY GP5106F PC/ABS+GF10%, Flame Retardance Description: Injection Molding, PC/ABS+GF10%, Flame RetardanceApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 235 °C | 428 - 455 °F | Start Point: 230°C |
Kingfa MAC-501DY Modified PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa PA6-RG30 Flame Retardant, 30% Glass Fiber Reinforced PA6 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesApplications:Injection moldingConnectorsRelayBobbinsPlugsInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa PBT-R0N Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa PBT-RG151 Flame Retardant, 15% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesExcellent size stabilityNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInforma.. |
|||
Rear Barrel Temperature | 220 - 275 °C | 428 - 527 °F | Injection Molding |
LG Chemical LUPOY GN5001RFD PC/ABS, High Impact Description: Injection Molding, PC/ABS, General Purpose, High Impact, Halogen Free Flame retardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUPOY GP1000LG PC, Transparent Description: Injection Molding, PC, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsInformation provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 225 °C | 428 - 437 °F | |
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr.. |
|||
Rear Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Aft-1. Region Temperature |
Tisan TISESTER® 15% Glass Fiber Reinforced Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Rear Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Aft-1. Region Temperature |
Tisan TISESTER® 30% Glass Fiber Reinforced and heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 15% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 30% Glass Bead Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 UNR Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 220 - 230 °C | 428 - 446 °F | Zone 1 |
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |