Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
Multibase Multi-Pro® 1020 C Polypropylene Calcium Carbonate Filler, 10% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
Multibase Multi-Pro® 2518 CU Polypropylene Calcium Carbonate Filler, 25% by weight.Features:Gloss, High Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
Multibase Multi-Pro® 5014 CUW Polypropylene Calcium Carbonate Filler. Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT2600-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Interior trimSplash shieldsStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT3080-425 Thermoplastic Polyolefin, UV Stabilized, YBWA Platinum Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT3080-757UV Thermoplastic Polyolefin, UV Stabilized, Pueblo Gold Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT3080-81 Thermoplastic Polyolefin, UV Stabilized, ACRA Titanium Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P100-01 Polypropylene Homopolymer, Black Applications: Wire harnessesTrim componentsUnderhood applicationsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P252-00 Polypropylene Copolymer, Natural Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P252-01 Polypropylene Copolymer, Black Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P252-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P254-00 Polypropylene Copolymer, Natural Applications: Air ducts - distributionInterior trimI/P componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P257-00 Polypropylene Copolymer, Natural Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products UVFT3082-74 Thermoplastic Polyolefin, 135K Flexural Modulus, UV Stabilized, Exterior DX9 Black Applications: Step padsHitch padsExterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
Polymer Resources ABS-GP1 General Purpose ABS General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Rear Barrel Temperature | 188 - 218 °C | 370 - 425 °F | |
Star Plastics ABS9020 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 188 - 218 °C | 370 - 425 °F | |
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 188 - 218 °C | 370 - 425 °F | |
Star Plastics ABSHFL Molding Grade ABS High Flow Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 188 - 218 °C | 370 - 425 °F | |
Star Plastics ABS3545 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have
an excellent soft t.. |
|||
Rear Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6060NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6060NC has an
excellent soft touch feel,.. |
|||
Rear Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,.. |
|||
Rear Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc.. |
|||
Rear Barrel Temperature | 188 °C | 370 °F | |
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |