Polymer Property : Rear Barrel Temperature = 132 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 132 - 171 °C
270 - 340 °F
PolyOne Dynaflex™ G2701-1000-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G2701-1000-02 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Good ..
Rear Barrel Temperature 132 - 171 °C
270 - 340 °F
PolyOne Dynaflex™ G2780-0001 Thermoplastic Elastomer (TPE)
Dynaflex™ G2780-0001 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmo..
Rear Barrel Temperature 132 - 171 °C
270 - 340 °F
PolyOne Dynaflex™ G2701C Thermoplastic Elastomer (TPE)
Dynaflex™ G2701C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Rubbery Feel..
Rear Barrel Temperature 132 - 171 °C
270 - 340 °F
PolyOne Dynaflex™ G2780C Thermoplastic Elastomer (TPE)
Dynaflex™ G2780C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmold A..