Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3011-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3040-55A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3040-70A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3040-85A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3340-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
LATI Latigea B01 F1 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
LATI Latigea B01 L/07 Bio-Polymer Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
LATI Latigray 37 B01-01 CX/35 Bio-Polymer Radiopaque compound based on Bio-Polymer (PLA, PHB, ...). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BC142MO Polypropylene Copolymer BC142MO is a controlled rheology polypropylene heterophasic copolymer. It is characterized by high impact strength, good stiffness, excellent process ability, good flow properties and low warpage. .. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BD310MO Polypropylene Copolymer BD310MO is a heterophasic copolymer. This grade is characterized by an optimum combination of good impact strength and very high stiffness. This grade is mildly nucleated to maximize the mechanical.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BD950MO Polypropylene Copolymer BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BF330MO Polypropylene Copolymer BF330MO is a heterophasic copolymer. This polymer is characterized by an optimum combination of high stiffness, high impact strength and good flow properties. This grade is designed for high-speed i.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | actual surface temp |
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS1000 Polymer, Natural Durastar DS1000 polymer has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to aromatic oils often causes c.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS1110UVI Polymer, Natural Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS1900HF Polymer, Natural Durastar DS1900HF polymer is a high flow grade of Durastar . Durastar DS1900HF flow lengths are increased 20-40% relative to Durastar DS1000 as shown by spiral flow testing. Other outstanding featur.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS1910HF Polymer, Natural Durastar DS1910HF polymer is a high flow grade of Durastar that contains a mold release. Durastar DS1910HF flow lengths are increased 20-40% relative to Durastar DS1010 as shown by spiral flow testi.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar MN610 Polymer, Natural Durastar MN610 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN610 has very .. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman Eastar BR001 Copolyester Eastar BR001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman Eastar DN004HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN004HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Eastman Eastar EN010 Copolyester Eastar copolyester EN010 is used primarily in molded thick wall European applications.Applications/UsesPackagingInjection moldingContainers |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Eastman Eastar MN021 Copolyester Eastar copolyester MN021 is a thermoplastic condensation copolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® 2533 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 2533 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® 2533 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 2533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® 2533 SD 02 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 2533 SD 02 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SD grade is heat and UV stabilized and contains mold release additive.Infor.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® 3533 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 3533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® 4033 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
LATI Latimass 37 B01-01 D025 Bio-Polymer Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |