Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 100 Thermoset Polyester, GP BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1403 Electrical Grade BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1902 Mineral Filled Alkyd BMC 1902 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression molding. It was developed primarily for applications requiring very good impact and flex.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 501E Mineral Filled, Glass Reinforced Polyester BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 5209 Mineral Filled, Glass Reinforced Polyester BMC 5209 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium .. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 600LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600LS molding compound is a low-shrink, Mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose materia.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 610 Mineral filled, glass-fiber-reinforced polyester compound BMC 610 molding compound is a mineral filled, glass fiber reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is set a part form other medium impact.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 680 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression and stuffer injection molding It is characterized by good moldability, very high impa.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 685 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, oil .. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 880 Medium Strength Molding Compound BMC 880 is a medium strength, low shrink molding compound designed for outdoor applications. This material is UL Listed 94-V0/5V and is UL approved for outdoor use. It can be supplied in bulk or ext.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 901 Encapsulating Grade Molding Compound BMC 901 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A50-XHS Bulk molding compound Description: BMC A50XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in preweighted slugs. Due to the excellent flow and controlled reactivity, BMC A50XHS i.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A50-XHS-U Bulk molding compound Description: BMC A50-XHS-U is a high strength bulk molding compound with a UL F1 rating for outdoor exposure. This material was specifically designed for outdoor lighting and electrical applications.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1000 Thermoset Polyester, Food Grade BMC 1000 is a general purpose, food contact grade, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. As with all other BMC, Inc. compounds, .. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1412 Flame and Track Resistant BMC 1412 is an extremely versatile material. Flame and track resistant, low shrink for close dimensional control and surface smoothness, high physical properties. Developed for injection molding, bu.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1423 Wear Resistant, Electrical Grade BMC 1423 is a wear-resistant electrical grade material used in applications where there are moving parts. Best anti-wear properties are exhibited when used in conjunction with mating parts molded fr.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 2201 Mineral Filled Alkyd BMC 2201 molding compound is a mineral filled, glass-fiber-and nylon-floc reinforced alkyd compound suitable for compression and transfer molding. It was developed for applications requiring better .. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 5209-12940 Mineral Filled, Glass Reinforced Polyester BMC 5209-12940 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 610 Mineral Filled, Glass Reinforced Polyester Compound BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620M molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by high impact strength, good mol.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 8005 Polyester Molding Compound |