Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 82.2 - 121 °C | 180 - 250 °F | |
PolyOne Gravi-Tech™ GRV-PS-027-BA-WHT Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Mold Temperature | 91.0 - 121 °C | 196 - 250 °F | |
Covestro Petlon® 7530 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperat.. |
|||
Mold Temperature | 82.2 - 121 °C | 180 - 250 °F | Average value: 103 °C Grade Count:3 |
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and m.. |
|||
Mold Temperature | 65.6 - 121 °C | 150 - 250 °F | Average value: 93.3 °C Grade Count:8 |
Overview of materials for Polycarbonate, Aramid Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Mold Temperature | 65.6 - 121 °C | 150 - 250 °F | Average value: 106 °C Grade Count:10 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Mold Temperature | 60.0 - 121 °C | 140 - 250 °F | Average value: 90.1 °C Grade Count:106 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Mold Temperature | 93.0 - 121 °C | 199 - 250 °F | |
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Mold Temperature | 82.2 - 121 °C | 180 - 250 °F | |
Entec Hylox® 9030 PBT, 30% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Mold Temperature | 82.2 - 121 °C | 180 - 250 °F | |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Mold Temperature | 93.3 - 121 °C | 200 - 250 °F | |
Clariant Renol BR2065 Nylon 66, Mineral/Glass Reinforced Data provided by Clariant Masterbatches |
|||
Mold Temperature | 38.0 - 121 °C | 100 - 250 °F | Average value: 92.1 °C Grade Count:72 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |