Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 82.2 - 104 °C | 180 - 219 °F | |
PolyOne Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Mold Temperature | 48.9 - 104 °C | 120 - 219 °F | |
LNP Lubricomp® PDX-U-95672 BK8-115 Polyphthalamide, Proprietary Filler
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Mold Temperature | 71.1 - 104 °C | 160 - 219 °F | Average value: 88.6 °C Grade Count:3 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Mold Temperature | 71.0 - 104 °C | 160 - 219 °F | |
Styron EMERGEâ„¢ 4510-15 Polycarbonate EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform.. |
|||
Mold Temperature | 71.0 - 104 °C | 160 - 219 °F | |
Styron EMERGEâ„¢ 4530-10 Polycarbonate EMERGEâ„¢ PC 4530-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform.. |
|||
Mold Temperature | 71.0 - 104 °C | 160 - 219 °F | |
Styron EMERGEâ„¢ 4800-10 Polycarbonate EMERGEâ„¢ 4800-10 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
Mold Temperature | 71.0 - 104 °C | 160 - 219 °F | |
Styron EMERGEâ„¢ 4850-10 Polycarbonate EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Mold Temperature | 71.0 - 104 °C | 160 - 219 °F | |
Styron EMERGEâ„¢ 4510-10 Polycarbonate EMERGEâ„¢ PC 4510-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform.. |
|||
Mold Temperature | 71.0 - 104 °C | 160 - 219 °F | |
Styron EMERGEâ„¢ 4530-15 Polycarbonate EMERGEâ„¢ PC 4530-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co.. |
|||
Mold Temperature | 82.0 - 104 °C | 180 - 219 °F | |
Elastocon TPE Technologies Elastocon® STK55PA Thermoplastic Elastomer Elastocon® STK55PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK55PA is well suited for consumer go.. |
|||
Mold Temperature | 82.0 - 104 °C | 180 - 219 °F | |
Elastocon TPE Technologies Elastocon® STK56PA Thermoplastic Elastomer Elastocon® STK56PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA is well suited for consumer go.. |