Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.0 - 85.0 °C | 149 - 185 °F | |
PolyOne LubriOne™ AS-000/15T Acrylonitrile Butadiene Styrene (ABS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Mold Temperature | 65.0 - 85.0 °C | 149 - 185 °F | |
PolyOne Stat-Tech™ AS-15CF/000 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Mold Temperature | 65.0 - 85.0 °C | 149 - 185 °F | |
PolyOne Bergamid™ B70 G/GK30 TM-Y UV NC Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Mold Temperature | 65.0 - 85.0 °C | 149 - 185 °F | |
PolyOne Bergamid™ B70 G30 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Mold Temperature | 50.0 - 85.0 °C | 122 - 185 °F | Average value: 70.6 °C Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Mold Temperature | 27.0 - 85.0 °C | 80.6 - 185 °F | Average value: 65.4 °C Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Mold Temperature | 62.8 - 85.0 °C | 145 - 185 °F | Average value: 73.9 °C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Mold Temperature | 65.0 - 85.0 °C | 149 - 185 °F | Injection |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Mold Temperature | 60.0 - 85.0 °C | 140 - 185 °F | |
BASF Ultramid® BU50I PA6 (Dry) Description: Ultramid Ultratough Nylon BU50I is an unreinforced PA6, impact modified injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme .. |