Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Plastcom PLASTAMID® 66 BT N 27 B/IM PA66 PA66 for injection molding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, cla.. |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | |
Plastcom SLOVAMID 6 G 5 Polyamide 6, 5% Graphite FeaturesPA 6 for injection moulding with addition of 5% graphite, the PA surface rolling resistance force is significantly lowered. Used mainly in the product of crates and cases for bearings, slid.. |
|||
Mold Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Plastcom SLOVAMID 6 GF 10 TS PA6, 10% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Polykemi AB POLYabs V0X ABS, Flame Retardant Information provided by Polykemi AB |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE.. |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
Polykemi AB POLYfill PPC T1030 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
Polykemi AB POLYfill PPH T4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
Polykemi AB POLYfill PPH GF4030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
Polykemi AB POLYfill PPH T20020 UV Polypropylene Homopolymer, Mineral Reinforced, UV-Stabilized Information provided by Polykemi AB |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
Polykemi AB POLYfill PPH T4060 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | 80°C is Preferred |
Nilit Nilamid A3 H ZE High Impact PA66 Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength.. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Idemitsu Kosan Xarec® N WA 7010 SPS, 10% Glass Filled
(discontinued **) Crystalline Polymer Blend, Glass Filled. Used in Automotive Electronics applications. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
LATI LATAMID 12 H FE85 Nylon 12 Base Magnetizable Compound
(discontinued **) Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us.. |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
LG Chemical EF-378 ABS, Flame Retardant, Halogen Free Information Provided by LG Chem |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Start Point: 70°C |
Kingfa MAC-601 DY Modified 60/40 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelPower toolComputer and acce.. |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | Injection Molding |
LG Chemical LI911 ASA Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | Injection Molding |
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG.. |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
LG Chemical NS-161 ABS, Antistatic, High Strength Information Provided by LG Chem |
|||
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F | Start Point: 60°C |
Kingfa PBT-RG002 Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Injection Molding |
LG Chemical Lupox® GP2306FY PBT+GF30% Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided .. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Covestro Makroblend® DP UT3907 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT3907* offers superior flowability, good impact strength and excellent ch.. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Covestro Makroblend® KU 2-7608 Polycarbonate + PBT, Mineral Filled Impact Grade ISO 7792-1-PC/PBT,MHPR,-030,MD10(PC+PBT)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Eurostar Staramide BS6 PA6, 30% Glass Bead Filled, Injection Molded Staramide BS6 is a 30% Glass Bead Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Eurostar Staramide BG6 PA6, 30% Glass Filled, Injection Molded BG6 is a 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
E-Polymers TEKAMID® H12TW Unreinforced Low warpage PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Beijing Chemical Industry KAIFA® HN301-M30 PA6 Resin Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
Polykemi AB POLYfill PPH TS4040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
E-Polymers Tekaloy® S630X , High Impact, Weather Resistance, Chemical Resistance PC/PBT Alloy High impact, weather resistance, chemical resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | Injection-molding |
BASF Ultramid® B3L PA6 (Conditioned) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |