Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom PLASTALEN® EH 91 N Polyethylene HDPE regrind for injection molding. General use in all industry branches. Delivered in blue ( approx. RAL 5015) mode.Information Provided by Plastcom spol. s r.o. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom PLASTALEN® TPU N 85 LTS TPU Modified TPU. Use in all industry sectors. Delivered in the black.Information Provided by Plastcom spol. s r.o. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN EQ 71 N PP, imp. strength FeaturesPE modified with EVA. The addition of EVA causes increased toughness. General application in all industry branches. Delivered in natural mode and in the full RAL colour scale.Packaging, tran.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PC 59 GB 10 PP, 10% glass beads FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass beads and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | |
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE) OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | |
PolyOne OnFlex™ S EF 60A-3S1967 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
PolyOne OnFlex™ S KA 80A-3S1770 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
PolyOne OnFlex™ S KG 80A-3E2020 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | |
PolyOne OnFlex™ U 5370A-S0015 Thermoplastic Elastomer (TPE) OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | |
PolyOne OnFlex™ U 5470A-E0083 Thermoplastic Elastomer (TPE) OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5400 series are based upon alloys of SEBS and aliphatic TPU, combining the adv.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complica.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® SK645FR BK851 PBT
(Unverified Data**) Crastin® SK645FR BK851 is a flame retardant , 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.75mm.Information provided by DuPont Performance P.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | Start Point: 50°C |
Kingfa HF-606 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowModerate UV stabilityHigh stiffnessApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co.,.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | Injection molding |
LG Chemical KEYFLEX TO-1075A Thermoplastic Olefin for Injection Molding, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | Injection Molding |
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Mold Temperature | 30.0 - 65.6 °C | 86.0 - 150 °F | |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Mold Temperature | 30.0 - 65.6 °C | 86.0 - 150 °F | |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Daplen™ ED230HP Polypropylene TPO Compound Daplen™ ED230HP is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis GB311U Polypropylene Compound, Glass Fiber Reinforced GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Mold Temperature | 30.0 - 65.6 °C | 86.0 - 150 °F | |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Mold Temperature | 30.0 °C | 86.0 °F | Injection Molding |
Covestro Texin® 185 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialSc.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Eurostar Starflam M10009XP PP, Flame Retardant, Injection Molding Starflam M10009XP is an Unfilled Flame Retardant Polypropylene (Copolymer) Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 30.0 - 150 °C | 86.0 - 302 °F | |
E-Polymers SEPAZ® C230GP 30% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Mold Temperature | 30.0 - 40.0 °C | 86.0 - 104 °F | |
Carmel Olefins CAPILENE® QW 73 AV Propylene Random Copolymer Description: CAPILENE® QW 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QW 73 AV is clarified with antista.. |
|||
Mold Temperature | 30.0 °C | 86.0 °F | Injection Molding |
Covestro Texin® 255 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PH 91 N Polypropylene Homopolymer FeaturesModified homopolymer PP for injection moulding. General use in all industry branches - packing material, garden flower-pots, toys, furniture industry, hinges, fasteners, clamps, office chai.. |
|||
Mold Temperature | 30.0 - 150 °C | 86.0 - 302 °F | |
E-Polymers SEPAZ® C130M 30% Mineral Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Mold Temperature | 30.0 - 100 °C | 86.0 - 212 °F | suitable temperature 40-60°C |
Gromax CCP PBT 1200-211E Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |