Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
PolyOne OnFlex™ S KE 50A-3S1731 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Polykemi AB POLYelast TPE S902A Thermoplastic Elastomer, SBS-based Information provided by Polykemi AB |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Polykemi AB POLYelast TPE ZS706 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Termopol Termoton® K2GA4065A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Termopol Termoton® K2GA5080A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Termopol Termoton® K6GA4040A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Termopol Termoton® V2GA0065A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Premix Thermoplastics PRE-ELEC® PE 1270
(discontinued **) PRE-ELEC PE 1270 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 12.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | Injection Molding |
LG Chemical KEYFLEX BT HB9242D Ester Type TPE Description: TPC-ET, Blow Moldable, Low Modulus, Black ColorApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
SK Chemicals SKYTHANE® CS195A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
SK Chemicals SKYTHANE® R155D Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
SK Chemicals SKYTHANE® S368D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
SK Chemicals SKYTHANE® T875A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
SK Chemicals SKYTHANE® S180A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Covestro Desmopan® DP 2590A Polyurethane Extrusion- and injection molding gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationBlown filmsPreprocessingMax. Water content.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Covestro Desmopan® DP 3491A Polyurethane Extrusion- and injection molding gradesuitable for extrusion blow moldinghigh mechanical strengthhigh melt stabilityApplicationBlow moldingProfilesInjection molded engineering partsPreprocessingMax... |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Covestro Desmopan® DP 6065A Polyurethane injection molding gradefree from plasticizersvery good hydrolysis and microbial resistancevery short cycle timesApplicationhard - soft systemsShoe solesPreprocessingMax. Water content |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Eurotec® Tecolen® CP10 GR10 NL PPCP, 10% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Eurotec® Tecolen® CP30 NL XC30 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 20.0 - 80.0 °C | 68.0 - 176 °F | |
Arkema Group Rilsan® Clear G380 Renew Polyamide Rilsan® Clear G830 Rnew is a high performance transparent polyamide partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan 564 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and a high abrasion resistance.Typical Applications: Heel top-pieces, castor tyres and parts requiri.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan B 60 A ESD TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan SP 852 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan 664 DU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Polykemi AB POLYfill PP 150ENH Polypropylene, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan S 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |