Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 163 - 218 °C | 325 - 425 °F | Average value: 190 °C Grade Count:13 |
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and .. |