Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 3540 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go.. |
|||
Mold Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 7321 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantUV Resistance, Good Processability, Good.. |
|||
Mold Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 9002 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Mold Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 9002 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Mold Temperature | 51.7 °C | 125 °F | |
Multibase Multi-Flex® A 9402 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Mold Temperature | 51.7 - 79.4 °C | 125 - 175 °F | |
Clariant 6008 L Nylon 6, High Impact, Injection Molding Data provided by Clariant Masterbatches |
|||
Mold Temperature | 51.7 - 79.4 °C | 125 - 175 °F | |
Clariant Renol CAB1000 Cellulose Acetate Butyrate Data provided by Clariant Masterbatches |
|||
Mold Temperature | 51.7 - 79.4 °C | 125 - 175 °F | |
Clariant Renol PA2SP0017 Nylon 6, Impact Modified Data provided by Clariant Masterbatches |
|||
Mold Temperature | 51.7 - 65.6 °C | 125 - 150 °F | |
Clariant Renol PPSP0004 Polypropylene, Random Copolymer Data provided by Clariant Masterbatches |
|||
Mold Temperature | 51.7 - 79.4 °C | 125 - 175 °F | |
Clariant Renol PPSSP0001 Polyphenylene Sulfide, Glass Fiber and Bead Filled Data provided by Clariant Masterbatches |