Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 40.6 - 71.1 °C | 105 - 160 °F | |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Mold Temperature | 40.6 - 71.1 °C | 105 - 160 °F | |
Ravago Manufacturing Americas Hylac® FR74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Mold Temperature | 40.6 - 79.4 °C | 105 - 175 °F | Injection Molding |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Mold Temperature | 40.6 - 79.4 °C | 105 - 175 °F | |
DuPont Surlyn® SG201U NC010 Supergloss Molding Alloy Surlyn® SG201U is a modified ionomer resin for applications that require a high gloss, molded in color surface color surface finish directly from the mold. The material is weatherable, durable, an.. |