Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 18.0 - 75.0 °C | 64.4 - 167 °F | |
Lavergne VYPET VNT 1020 Polyester-PC Alloy The Vypet 1020 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Mold Temperature | 18.0 - 75.0 °C | 64.4 - 167 °F | |
Lavergne VYPET VNT 1021 Polyester-PC Alloy The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |