Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 2006 T Polypropylene Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 3018 TU Polypropylene Talc Filled, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Automotive Under the HoodInformation provided by Multibase |
|||
Mold Temperature | 4.44 - 65.6 °C | 40.0 - 150 °F | |
Multibase Multi-Pro® 5014 CUW Polypropylene Calcium Carbonate Filler. Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase |
|||
Mold Temperature | 37.8 - 65.6 °C | 100 - 150 °F | |
Fiberfil® J-69/10/E High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 37.8 - 65.6 °C | 100 - 150 °F | |
Fiberfil® J-69/40/E High performance polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® OBC 4864A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL EF-6155 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1336 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1336A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-2555F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-2635A Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-2683B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Mold Temperature | 43.3 - 65.6 °C | 110 - 150 °F | |
Calsak CS-72 General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |