Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Gravi-Tech™ GRV-TE1-060-W-NAT Styrene Isoprene Styrene Block Copolymer (SIS) Information provided by PolyOne |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Gravi-Tech™ GRV-TP-080-W-NAT Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Versaflex™ CL30 Thermoplastic Elastomer (TPE) Versaflex™ CL30 is an easy processing compound designed for use in injection molding and extrusion applications where water-clarity and excellent colorability are required. - Excellent Clarity - Ex.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE) Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora.. |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
PolyOne Versaflex™ OM 9-801N Thermoplastic Elastomer (TPE) Versaflex™ OM 9-801N is designed for overmolding onto a wide variety of substrates including PC, ABS, PC/ABS, HIPS, PPO, acetal, acrylic and copolyester. - Bonds to a Variety Of Substrates - Rubber.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7930-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7930-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® 2890 Thermoplastic Elastomer Elastocon® 2890 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2890 is FDA compliant and well suited for cons.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.0 - 100 °F | |
PolyOne Edgetek® UR-30GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |