Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-G33 Nylon 66, 33% Glass Reinforced Nylon 66, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | |
Polymer Resources NY66-IM1-G13 Nylon 66, 13% Glass Reinforced, Toughened Nylon 66, 13% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-IM2-G33 Nylon 66, 33% Glass Reinforced, Impact Modified Nylon 66, 33% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | |
Polymer Resources NY66-M25G15-[color]-H Nylon 66, 25% Mineral, 15% Glass Reinforced, Heat Stabilized Nylon 66, 25% Mineral, 15% Glass Reinforced, Lubricated and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, te.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY6-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced Modified-Polyphenylene Oxide, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | thick wall - thin wall |
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled
(discontinued **) Information provided by MRC Polymers Inc. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-G33-[color]-H Nylon 66, 33% Glass Reinforced, Heat Stabilized Nylon 66, 33% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-G43-[color]H Nylon, 43% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-IMG33-[color]H Nylon, 33% Glass Reinforced, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | |
Polymer Resources NY6-G43-[color]-H Nylon 6, 43% Glass Reinforced, Heat Stabilized Nylon 6, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | |
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Mold Temperature | 71.0 - 104 °C | 160 - 219 °F | |
Styron EMERGEâ„¢ 4510-15 Polycarbonate EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | |
Clariant Renol PCSP0004 Polycarbonate Alloy Data provided by Clariant Masterbatches |
|||
Mold Temperature | 93.3 - 104 °C | 200 - 220 °F | |
PolyOne Lubri-Tech™ NI-30CF/10T-2S Nylon 6/10, Carbon Fiber Reinforced, PTFE/Silicone Lubricated
(discontinue Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
Polymer Resources PPX-G20 Modified PPO, 20% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |