Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova PS 3190 Crystal Polystyrene
(discontinued **) Information provided by Nova ChemicalsINEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 1210 High Heat Crystal Polystyrene
(discontinued **) High heat resistance, High molecular weight, optimum performance in extruded foamApplications: Meat and poultry trays, Egg cartons, Food packagingExposure to gamma radiation in the 2.02-6.06 megarad.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 1230 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 1531 High Heat Crystal Polystyrene
(discontinued **) High flow and high heat resistance, Excellent clarityApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical p.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 2110 General Purpose Crystal Polystyrene
(discontinued **) Moderately high heat resistance, Good balance of strength and ease of processing, USP Class VIApplications: Foam extrusion, Biaxially oriented sheet, Thermoformed drinkware, Molded packagingExposure.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 3900 General Purpose Crystal Polystyrene
(discontinued **) High flow, Good compoundingApplications: Color concentrates, Compounding, Thin wall moldingsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and o.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
PolyOne Stat-Tech™ AS-7SS/000 ABS - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 1290 High Heat Crystal Polystyrene Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 1510 High Heat Crystal Polystyrene High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5400 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5410 High Impact Polystyrene High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverages cups, Custom sheetProperties were determined on injection molded specimens at 23°C .. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5511 High Impact Polystyrene Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova FX530 Impact Polystyrene Features: Excellent environmental stress crack resistanceExcellent Izod impact strengthUL Classification 94 HBBalanced physical propertiesApplications: ExtrusionThermoformingSelected injection moldi.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan LX201 Copolyester Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan MX710 Copolyester Eastman Tritan Copolyester MX710 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX710 has many outstanding features that include excellent toughness, hydr.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan MX730 Copolyester Eastman Tritan Copolyester MX730 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX730 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan MX810 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceOutstanding impact re.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan TX2000 Copolyester Eastman Tritan TX2000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 3510 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5420 High Impact Polystyrene
(discontinued **) High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection m.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5450 High Impact Polystyrene
(discontinued **) High impact, Good ESCRApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were determined on injection molded specimens at 23.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5540 High Impact Polystyrene
(discontinued **) Excellent balance of toughness, flow, and set-up, High gloss, USP Class VIApplications: Structural foam, Housewares, Toys, Appliance parts, Dairy containersProperties were determined on injection mo.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5711 High Impact Polystyrene
(discontinued **) High flow, High impact, USP Class VIApplications: Thin wall, Medical, Housewares, ToysProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Inform.. |
|||
Mold Temperature | 38.0 °C | 100 °F | |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Mold Temperature | 38.0 °C | 100 °F | |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 1301 High Heat Crystal Polystyrene High heat resistance, High strength, Good processing characteristics, USP Class VIApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5530 High Impact Polystyrene
(discontinued **) Good overall balance of properties, Good toughnessApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C.. |
|||
Mold Temperature | 38.0 - 79.0 °C | 100 - 174 °F | |
Samsung Cheil Industries Starex® HF-5661H ASA, Unreinforced
(discontinued **) Amorphous Styrene Acrylonitrile (SAN)Characteristics: High Flow: Impact, Heat and Chemical Resistance and Surface GlossApplications: Pens, TV Components, Refrigerator and Appliance ComponentsProcess.. |