Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 37.8 - 43.3 °C | 100 - 110 °F | |
Northstar Polymers MPP-R07B Polyurethane Formulation This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is long enough to allow manual handling for cast-.. |
|||
Mold Temperature | 37.8 - 82.2 °C | 100 - 180 °F | |
Polymer Resources PPX-SF1 Modified-PPO, Structural Foam Grade, Flame Retardant, Easy Flow Modified-Polyphenylene Oxide, Structural Foam Grade, Easy FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechani.. |
|||
Mold Temperature | 37.8 - 51.7 °C | 100 - 125 °F | |
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Mold Temperature | 37.8 - 65.6 °C | 100 - 150 °F | |
Fiberfil® J-69/10/E/UV High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 37.8 - 93.3 °C | 100 - 200 °F | |
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled 13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 37.8 °C | 100 °F | |
Multibase Multi-Flex® D 6505 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInform.. |
|||
Mold Temperature | 37.8 - 65.6 °C | 100 - 150 °F | |
Fiberfil® J-69/20/E High performance polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 37.8 - 48.9 °C | 100 - 120 °F | |
Star Plastics ABS3030 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 37.8 - 65.6 °C | 100 - 150 °F | |
Ecomass® 705ZG91 Stainless Steel/Tungsten Filled ABS High Specific GravityStainless Steel/Tungsten Powder Filled ABSInformation provided by Technical Polymers |
|||
Mold Temperature | 37.8 - 82.2 °C | 100 - 180 °F | Higher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products. |
Diamond Polymers ASA S910 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Mold Temperature | 37.8 - 82.2 °C | 100 - 180 °F | Higher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products. |
Diamond Polymers ASA T-110 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Mold Temperature | 37.8 - 93.3 °C | 100 - 200 °F | |
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled 13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |