Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom PLASTALEN® PQ 81 N 003 Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | |
PolyOne OnFlex™ S EF 50A-3S1965 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
PolyOne OnFlex™ S HF 70A-3S1984 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
PolyOne OnFlex™ S KG 40A-3S2016 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
PolyOne OnFlex™ S KG 80A-3E2020 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Mold Temperature | 30.0 - 40.0 °C | 86.0 - 104 °F | |
Premix Thermoplastics PRE-ELEC® ESD 5350 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5350 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Mold Temperature | 30.0 - 70.0 °C | 86.0 - 158 °F | |
Premix Thermoplastics PRE-ELEC® ESD 7120 PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® 6134 NC010 PBT
(Unverified Data**) Crastin® 6134 NC010 is an unreinforced, medium viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Injection Molding |
DuPont Performance Polymers Crastin® S650FR BK851 PBT
(Unverified Data**) Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® SK645FR BK851 PBT
(Unverified Data**) Crastin® SK645FR BK851 is a flame retardant , 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.75mm.Information provided by DuPont Performance P.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PH 56 T FRD 1 PP, flame retardant FeaturesModified homopolymer PP for injection moulding with decreased flammability. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil forms, guides, co.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | Start Point: 50°C |
Kingfa FRHIPS-960 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingPrinter and photocopier .. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | Start Point: 50°C |
Kingfa HP-126 Modified ABS Features:UL94 HB @ 1.6-3.0mmHigh impact resistanceHigh flowApplications:LCD cabinetLarge thin-wall partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | Start Point: 50°C |
Kingfa HR-527A Modified ABS Features:UL94 HB @ 1.5-3.2mmHeat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | Injection Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | Start Point: 50°C |
Kingfa FRHIPS-8002 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.0mm, V-2 @ 3.2mmExcellent balancing properties, Non-DPOExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElec.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | Injection Molding |
Styrolution Terluran® HH-112 Q109 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Sumitomo Chemical ESPOLEX® 3885 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Sumitomo Chemical ESPOLEX® WT446 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Mold Temperature | 30.0 - 65.6 °C | 86.0 - 150 °F | |
A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy Information provided by A. Schulman. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis GB311U Polypropylene Compound, Glass Fiber Reinforced GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Mold Temperature | 30.0 - 65.6 °C | 86.0 - 150 °F | |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® S600LF NC010 PBT Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Eurostar Starpylen MF004S PP, 20% Glass Fiber Filled, Injection Molded Starpylen MF004S is a 20% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 30.0 - 40.0 °C | 86.0 - 104 °F | |
Carmel Olefins CAPILENE® QW 73 AV Propylene Random Copolymer Description: CAPILENE® QW 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QW 73 AV is clarified with antista.. |
|||
Mold Temperature | 30.0 - 90.0 °C | 86.0 - 194 °F | |
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | Injection Molding |
BASF Styroclear GH 62 SBC Styroclear GH 62 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Daplen™ EE103AE TPO Compound Daplen EE103AE is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE103AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |