Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 27.0 - 60.0 °C | 80.6 - 140 °F | |
Eastman Eastalloy DA510 Polymer
(discontinued **) Eastalloy Polymer DA510 is a clear copolyester/polycarbonate alloy. This product has good physical properties. These include good impact strength, chemical resistance, heat resistance, dimensional s.. |
|||
Mold Temperature | 27.0 - 60.0 °C | 80.6 - 140 °F | |
Eastman Eastalloy MA510 Polymer
(discontinued **) Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhan.. |
|||
Mold Temperature | 27.0 °C | 80.6 °F | |
Eastman Eastar Copolyester K3000 PETG Copolyester
(discontinued **) EASTAR K3000 Copolyester is a cost effective, high-performance, water-clear material that provides the necessary performance for the appliance standards. Other desirable characteristics are good ch.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 221 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: High clarityEnhanced mold releaseGood elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilization Applications: DisplaysMedical devicesOffice acc.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 390 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: Excellent clarityHigh flexural modulusGood toughness and elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specification.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 330 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Clarity and stiffness Good heat distortion resistance Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class .. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 220 High Performance Styrenic, Acrylic Copolymer
(discontinued **) Excellent moldability, High clarity, Extended toughness and elongation, meets USP XXI specification for Class VI Plastics, Property retention after gamma irradiationApplications: Display, medical de.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 1983 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Color Stable, Custom colors, UL94 HB at 0.060 for all colorsApplications: Suitable for extrusion or injection molding processes requiring.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 271 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Excellent balance of stiffness, heat resistance, and impact properties, Custom colorsApplications: Injection molding and extrusion, Applications requiring strength and durability where custom colori.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 50 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High strength crystal polystyrene, High heat crystal polystyrene, Custom colorsApplications: Injection molding or extrusion, Designed for applications requiring strength and high heat resistance whe.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 474 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Alternative to engineering resinsPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. N.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 1552 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Easy processing, High modulus, Improve stress whitening, Custom colorsApplications: Injection molding, Office furniture, Electronic media, Photographic equipmentPerformance grades of polystyrene are.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 850 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Custom colorsApplications: Injection molding or extrusion, Suitable replacement for some engineering resins, Toys, Packaging, Business eq.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 765 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, High impact, Color stable, Custom colorsApplications: High flow, multi-purpose injection molding grade where color stability is a requirement, Toys, Appliance, Computer peripheralsPerform.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 782 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Custom colorsApplications: Multi-purpose injection molding where custom color is a requirement, Toys, Appliance, Computer peripheralsPerformance grades of polystyrene are engineered to ha.. |
|||
Mold Temperature | 27.0 - 85.0 °C | 80.6 - 185 °F | Average value: 65.4 °C Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
PolyOne Edgetek® AS- 08CF / 000 ABS - 8% Carbon Fiber Reinforced With ESD Properties
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 27.0 - 49.0 °C | 80.6 - 120 °F | |
PolyOne Edgetek® AS-1000 SD Unreinforced ABS - Antistatic Protection
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
PolyOne Edgetek® AS-10CF/000 ABS - 10% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
PolyOne Stat-Tech™ AS-15GF/000 SD ABS - 15% Glass Fiber Reinforced - Antistatic Protection
(discontinued **)& Data provided by PolyOne. |
|||
Mold Temperature | 27.0 °C | 80.6 °F | |
Eastman Eastar GN071 Natural PETG Copolyester EASTAR GN071 Copolyester is used for injection molding applications. It is sparkling clear, tough, chemical resistant, odor free, versatile, easy to work with and affordable. Cleaning solutions wi.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 535 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: High clarity, strength and toughnessStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationAnti-stat packageEnhanced mold releaseUL 94HB @ 1.5 mm for a.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Outstanding practical toughness and ductilityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationUSP Class VI compliantCustom colors and enhancement .. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties.. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova 8049 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High gloss at 60°=95; at 20°C=90, Improved scuff resistance, Custom colorsApplications: Injection molding, Cost effective replacement for some ABS applications, Excellent for applications where hi.. |
|||
Mold Temperature | 27.0 - 107 °C | 80.6 - 225 °F | Average value: 61.1 °C Grade Count:39 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Mold Temperature | 27.0 - 54.0 °C | 80.6 - 129 °F | |
Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer
(discontinued **) Excellent heat distortion temperature, High clarity, strength and toughness, Enhanced mold releaseApplications: Industrial covers and housings, Paper towel dispenser covers, Appliance partsInjection.. |