Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE) Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Versaflex™ 9570-9 Thermoplastic Elastomer (TPE) Versaflex™ 9570-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Dynaflex™ G7930-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7960-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Mold Temperature | 15.6 - 70.0 °C | 60.0 - 158 °F | Average value: 47.5 °C Grade Count:20 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Mold Temperature | 15.6 - 76.7 °C | 60.0 - 170 °F | |
Green Dot Terratek® WC 100300 Polypropylene - Pine Fiber Composite Terratek® WC 100300 is a proprietary blend of pine wood fiber and reprocessed polypropylene for injection molding applications. WC 100300 contains 30% wood fiber by weight, however, a range of pr.. |
|||
Mold Temperature | 15.6 - 60.0 °C | 60.0 - 140 °F | |
DuPont Bexloy® AXW604BK 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin
(discontinued **) A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.0 - 100 °F | |
PolyOne Edgetek® UR-20GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |