Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 12.0 - 70.0 °C | 53.6 - 158 °F | Average value: 31.9 °C Grade Count:4 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Mold Temperature | 12.0 - 20.0 °C | 53.6 - 68.0 °F | Extrusion Blow Molding |