Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 320 - 350 °C | 608 - 662 °F | |
Solvay Specialty Polymers Primef® 5084 30% GF PPS, Lubricated Grade
(discontinued **) Contains PTFE lubricant. Used for injection molding of high performance parts. |
|||
Nozzle Temperature | 320 - 350 °C | 608 - 662 °F | |
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement
(discontinu Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu.. |
|||
Nozzle Temperature | 320 - 350 °C | 608 - 662 °F | |
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **) Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical.. |
|||
Nozzle Temperature | 320 - 350 °C | 608 - 662 °F | |
Solvay Specialty Polymers Primef® 7010 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **) Primef 7010 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers improved mechanical properties versus Primef 7002 (also 65% mineral/glass fiber), but with less flu.. |
|||
Nozzle Temperature | 300 - 350 °C | 572 - 662 °F | |
Hybrid Plastics PO6C81.01 Nanoreinforced® Polyphenylene Oxide (PPO) PPO available on the market today is typically mixed with polystyrene or other polymers to make it processable. However, these resins degrade the excellent mechanical and flammability properties of .. |
|||
Nozzle Temperature | 300 - 350 °C | 572 - 662 °F | |
LG Chemical LUCON PO-3000 Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Nozzle Temperature | 300 - 350 °C | 572 - 662 °F | |
LG Chemical LUCON PO-5300H Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Nozzle Temperature | 300 - 350 °C | 572 - 662 °F | |
LG Chemical LUCON PO-5300M Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Nozzle Temperature | 330 - 350 °C | 626 - 662 °F | |
Unitika P-3001S Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Nozzle Temperature | 330 - 350 °C | 626 - 662 °F | |
Unitika PT-3020 Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd. |
|||
Nozzle Temperature | 330 - 350 °C | 626 - 662 °F | |
Unitika P-3001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Nozzle Temperature | 320 - 350 °C | 608 - 662 °F | |
Solvay Specialty Polymers Primef® 4002 40% GF PPS, High Fluidity Grade
(discontinued **) Used for injection molding of high performance parts. |