Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 225 - 245 °C | 437 - 473 °F | Injection Molding |
LG Chemical KEYFLEX BT 1063D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 225 - 245 °C | 437 - 473 °F | Injection Molding |
LG Chemical KEYFLEX BT 1163D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 220 - 245 °C | 428 - 473 °F | Injection |
Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Nozzle Temperature | 220 - 245 °C | 428 - 473 °F | Injection |
Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Nozzle Temperature | 220 - 245 °C | 428 - 473 °F | Injection |
Kolon DIAMAT® GP Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Nozzle Temperature | 220 - 245 °C | 428 - 473 °F | Injection |
Kolon DIAMAT® IG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Nozzle Temperature | 220 - 245 °C | 428 - 473 °F | Injection |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Nozzle Temperature | 220 - 245 °C | 428 - 473 °F | Injection |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Nozzle Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUPOS GP2205 SAN+GF20%, General Purpose Feature: Injection Molding, SAN+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b.. |
|||
Nozzle Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance Feature: Injection Molding, ABS+GF20%, General Purpose, Heat ResistanceApplication: Electric & Electronic (Housing, Components)Information provided by LG Chemical |
|||
Nozzle Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® GP-1006F General Purpose PBT, Unreinforced, Flame Retardant, Non-Bleed LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Nozzle Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® GP-2000 General Purpose PBT, Unreinforced, Medium Viscosity LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Nozzle Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® SV-1080 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Nozzle Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® SV-1120 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Nozzle Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® GP-1001F General Purpose PBT, Unreinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Nozzle Temperature | 240 - 245 °C | 464 - 473 °F | |
Beijing Chemical Industry KAIFA® HN201-G20 PA6 Resin 20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 240 - 245 °C | 464 - 473 °F | |
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin 10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 240 - 245 °C | 464 - 473 °F | |
Beijing Chemical Industry KAIFA® HN301-G20 PA6 Resin 20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 240 - 245 °C | 464 - 473 °F | |
Beijing Chemical Industry KAIFA® HN301-G30 PA6 Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 210 - 245 °C | 410 - 473 °F | Injection Molding |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Nozzle Temperature | 210 - 245 °C | 410 - 473 °F | Injection Molding |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Nozzle Temperature | 240 - 245 °C | 464 - 473 °F | |
Beijing Chemical Industry KAIFA® HN201-G10 PA6 Resin 10% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 220 - 245 °C | 428 - 473 °F | Average value: 233 °C Grade Count:3 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Nozzle Temperature | 210 - 245 °C | 410 - 473 °F | Injection Molding |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Nozzle Temperature | 210 - 245 °C | 410 - 473 °F | Injection Molding |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |