Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 200 - 240 °C | 392 - 464 °F | Injection Molding |
LG Chemical KEYFLEX TO1192A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical |
|||
Nozzle Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LG703W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided.. |
|||
Nozzle Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical LUPOL TE-5108 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Flow LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by .. |
|||
Nozzle Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical LUPOL GP-3152F General Purpose Polypropylene, 15% Mineral Fillers, High Impact, Flame Retardant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Nozzle Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical LUPOL GP-3154F General Purpose Polypropylene, 15% Mineral Fillers, High Modulus, Flame Retardant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Nozzle Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical LUPOL HF-3202D High Flow Polypropylene, 20% Mineral Fillers, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Nozzle Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical LUPOL HM-4354 Heat Resistant Polypropylene, 35% Glass Fiber/Mineral Filler Reinforced, High Strength, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Nozzle Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Nozzle Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay TECHNYL® C 216 V15 PA6, 15% glass filled, Eh 0 Description: TECHNYL C 216 V15 is a polyamide 6 with 15% of glass fiber.Colors: it is marketed in the black color and natural.Available in: Asia Pacific and EuropeMain Properties: Dimensional stabil.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | |
Samyang Tribit® 1500 Polybutylene Terephthalate Characteristics:Medium viscosityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samy.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | |
Samyang Tribit® 1503 Polybutylene Terephthalate Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid.. |
|||
Nozzle Temperature | 180 - 240 °C | 356 - 464 °F | |
Arkema Group Pebax® 2533 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 2533 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Nozzle Temperature | 180 - 240 °C | 356 - 464 °F | |
Arkema Group Pebax® 3533 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 3533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Nozzle Temperature | 200 - 240 °C | 392 - 464 °F | Injection |
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Nozzle Temperature | 200 - 240 °C | 392 - 464 °F | Injection Molding |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Nozzle Temperature | 210 - 240 °C | 410 - 464 °F | Injection |
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Nozzle Temperature | 235 - 240 °C | 455 - 464 °F | |
Beijing Chemical Industry KAIFA® HN301-G0 PA6 Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 235 - 240 °C | 455 - 464 °F | |
Beijing Chemical Industry KAIFA® HN301-M30 PA6 Resin Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 200 - 240 °C | 392 - 464 °F | Injection Molding |
Arkema Group KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Nozzle Temperature | 200 - 240 °C | 392 - 464 °F | Injection Molding |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Nozzle Temperature | 180 - 240 °C | 356 - 464 °F | |
Arkema Group Pebax® Rnew 35R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 35R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Nozzle Temperature | 200 - 240 °C | 392 - 464 °F | Injection Molding |
LG Chemical KEYFLEX TO1088AV Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR401F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical |